GRP Fibreglass Flat Roofing: Installation Steps, Glass Mat Thickness, Topcoat Application and Common Defects
GRP installation: 450g/m² CSM, 1–2% MEKP catalyst, key coat timing (hardened but not fully cured), topcoat application, common defects (delamination, crazing, dry patches)